Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.15 J/cm² @Temperature -30.0 °C |
10.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Charpy Impact Unnotched | 2.15 J/cm² @Temperature -40.0 °C |
10.2 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |