Polymer Property : Charpy Impact Unnotched = 2.17 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.20 - 2.17 J/cm²
5.71 - 10.3 ft-lb/in²
Average value: 1.57 J/cm² Grade Count:5
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..