Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
ISO 179
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 3-7901 Polyamide 6, with glass fiber and carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific)
DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
ISO 179/1eU
Borealis Daplen™ FS65T20 Polypropylene Compound 20% Mineral Filled, Detergent Resistant
Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat sta..
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -30.0 °C
20.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4412 PC
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East)
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 4.30 J/cm²
20.5 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific)
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.