Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.70 J/cm²

@Temperature -30.0 °C
27.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact Unnotched 5.70 J/cm²

@Temperature -30.0 °C
27.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact Unnotched 5.70 J/cm²

@Temperature -30.0 °C
27.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 20-0664 Polyphthalamide, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific)
DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179/1eU
Borealis Nepol™ GB402HP 40% Long Glass Fiber Reinforced Polypropylene
Nepol GB402HP is a 40% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th..
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179-1
Unitika M1030DH PA6, Dry
Nano composite nylonInformation provided by Unitika Ltd.
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate  Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..
Charpy Impact Unnotched 5.70 J/cm²
27.1 ft-lb/in²
ISO 179/IeU
Addiplast Addilene PMD 50213 Polypropylene Copolymer
Mineral reinforced, improved scratch resistanceInformation provided by Addiplast.
Charpy Impact Unnotched 5.70 - 5.70 J/cm²

@Temperature -30.0 - -30.0 °C
27.1 - 27.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.70 J/cm² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..