Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.03 J/cm²

@Temperature 23.0 °C
28.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.