Polymer Property : Charpy Impact Unnotched = 3.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 - 3.60 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 17.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.63 J/cm² Grade Count:12
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..