Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.60 J/cm²
36.2 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Charpy Impact Unnotched 7.60 - 10.5 J/cm²

@Temperature -30.0 - 30.0 °C
36.2 - 50.0 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 8.93 J/cm² Grade Count:8
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Charpy Impact Unnotched 7.60 J/cm²
36.2 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Charpy Impact Unnotched 7.60 J/cm²
36.2 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Charpy Impact Unnotched 7.60 J/cm²

@Temperature -20.0 °C
36.2 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai..
Charpy Impact Unnotched 7.60 J/cm²

@Temperature 30.0 °C
36.2 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Charpy Impact Unnotched 7.60 J/cm²
36.2 ft-lb/in²
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Charpy Impact Unnotched 7.60 J/cm²

@Temperature -30.0 °C
36.2 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo..
Charpy Impact Unnotched 7.60 J/cm² - NB

@Temperature -40.0 - -30.0 °C
36.2 ft-lb/in² - NB

@Temperature -40.0 - -22.0 °F
Average value: 7.60 J/cm² Grade Count:4
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Charpy Impact Unnotched 7.60 J/cm²
36.2 ft-lb/in²
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform..
Charpy Impact Unnotched 7.60 J/cm²
36.2 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..