Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 37.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.80 J/cm²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY
Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ..
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, Conditioned
Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R..
Charpy Impact Unnotched 7.80 J/cm²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 CF 30 HWCP 30% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 7.80 J/cm²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 CF30 HWCP 30% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric..
Charpy Impact Unnotched >= 7.80 J/cm²

@Temperature 23.0 °C
>= 37.1 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
AKG Polymers Vision PP PPH BL1303 G30 Polypropylene Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
ISO 179
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN201-G30 PA6 Resin
30% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 7.80 J/cm²

@Temperature 23.0 °C
37.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled
Injection molding, heat stabilizedInformation provided by PolyPlastic Group.
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
BASF Novolen® 1148 UC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 7.80 J/cm²
37.1 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in..
Copyright © lookpolymers.com All Rights Reserved