Polymer Property : Charpy Impact Unnotched = 476 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 100 J/cm²
476 ft-lb/in²
ISO 179/1eU
Borealis Daploy™ WB130HMS High Melt Strength Polypropylene for Foam Extrusion
Daploy WB130HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g..