Polymer Property : Charpy Impact Unnotched = 52.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 11.1 J/cm²

@Temperature -30.0 °C
52.8 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No..