Polymer Property : Charpy Impact Unnotched = 6.47 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.600 - 1.36 J/cm²
2.86 - 6.47 ft-lb/in²
Average value: 0.889 J/cm² Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..