Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.69 J/cm²
31.8 ft-lb/in²
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..