Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.10 J/cm² @Temperature 23.0 °C |
43.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 9.10 J/cm² | 43.3 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Charpy Impact Unnotched | 9.10 J/cm² | 43.3 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 9.10 J/cm² | 43.3 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Charpy Impact Unnotched | 9.10 J/cm² @Temperature -30.0 °C |
43.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Conditioned) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |