Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 1150.8 MPa @Temperature 22.8 °C |
166910 psi @Temperature 73.0 °F |
Flexure Weft; 10 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle Information provided by HexCel |
|||
Flexural Yield Strength | 1150.8 MPa @Temperature 22.8 °C |
166910 psi @Temperature 73.0 °F |
Flexure Weft; 15 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle Information provided by HexCel |
|||
Flexural Yield Strength | 1150.8 MPa @Temperature 22.8 °C |
166910 psi @Temperature 73.0 °F |
Flexure Weft; 13 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF01 Epoxy Curing System after 1031 2 1000 970 EF01 31% Cure Cycle Information provided by HexCel |