Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 28.0 MPa @Temperature 316 °C |
4060 psi @Temperature 601 °F |
Autoclave Cured; [90°]16 |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |