Polymer Property : Flexural Yield Strength = 29200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 201 MPa

@Strain 3.50 %
29200 psi

@Strain 3.50 %
ISO 178
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers
PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized