Polymer Property : Flexural Yield Strength = 359.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 359.6 MPa

@Temperature 316 °C
52160 psi

@Temperature 601 °F
Press Cured; Tested at 316°C after 5-10 min at 316°C
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form
Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel