Mechanical Properties Metric English Comments
Flexural Yield Strength 260 MPa

@Strain 3.50 %
37700 psi

@Strain 3.50 %
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
Flexural Yield Strength 260 MPa

@Strain 3.50 %
37700 psi

@Strain 3.50 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.