Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 549 MPa @Temperature 90.0 °C |
79600 psi @Temperature 194 °F |
0°, Conditioning: 23°C; ASTM D790 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, AS4-C Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |