Mechanical Properties Metric English Comments
Flexural Yield Strength 552 MPa

@Temperature 177 °C
80100 psi

@Temperature 351 °F
T300; Fill Flexure; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel