Polymer Property : Flexural Yield Strength = 90.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 90.0 MPa

@Strain 3.50 %
13100 psi

@Strain 3.50 %
Conditioned; ISO 178
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
Flexural Yield Strength 90.0 MPa

@Strain 3.50 %
13100 psi

@Strain 3.50 %
Conditioned; ISO 178
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers
PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized
Flexural Yield Strength 90.0 MPa

@Strain 3.50 %
13100 psi

@Strain 3.50 %
Conditioned; ISO 178
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers
PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized