Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | >= 10.5 MPa | >= 1520 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 10.5 MPa | >= 1520 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |