Polymer Property : Creep Strength = 130 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength 130 MPa

@Temperature 600 °C,
Time 3.60e+6 sec
18900 psi

@Temperature 1110 °F,
Time 1000 hour
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se..