Mechanical Properties Metric English Comments
Creep Strength 120 MPa

@Temperature 600 °C,
Time 3.60e+6 sec
17400 psi

@Temperature 1110 °F,
Time 1000 hour
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel
Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b..
Creep Strength 120 MPa

@Temperature 600 °C,
Time 3.60e+6 sec
17400 psi

@Temperature 1110 °F,
Time 1000 hour
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi..