Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 2.068 MPa @Temperature 816 °C |
299.9 psi @Temperature 1500 °F |
0.0001% per hour |
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |