Polymer Property : Creep Strength = 3480 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength >= 24.0 MPa
>= 3480 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Dry
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
Creep Strength >= 24.0 MPa
>= 3480 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry
Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH