Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | >= 6.00 MPa | >= 870 psi | 1% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 6.00 MPa | >= 870 psi | 1% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 6.00 MPa | >= 870 psi | 1% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | 6.00 - 24.0 MPa | 870 - 3480 psi | Average value: 15.6 MPa Grade Count:15 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Creep Strength | 6.00 - 20.0 MPa | 870 - 2900 psi | Average value: 12.3 MPa Grade Count:6 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |