Polymer Property : Creep Strength = 124 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength 124 MPa

@Temperature 871 °C,
Time 360000 sec
18000 psi

@Temperature 1600 °F,
Time 100 hour
0.5% Creep
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Creep Strength 124 MPa

@Temperature 816 °C,
Time 3.60e+6 sec
18000 psi

@Temperature 1500 °F,
Time 1000 hour
0.5% Creep
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Creep Strength 124 MPa

@Temperature 871 °C,
Time 360000 sec
18000 psi

@Temperature 1600 °F,
Time 100 hour
1% Creep
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..