Mechanical Properties Metric English Comments
Creep Strength 22.0 MPa

@Time 3.60e+6 sec
3190 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
Creep Strength 22.0 MPa

@Time 3.60e+7 sec
3190 psi

@Time 10000 hour
in water at 95°C
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.