Mechanical Properties Metric English Comments
Creep Strength 64.43 MPa

@Temperature 538 °C
9345 psi

@Temperature 1000 °F
Crucible Steel 416 Plus Chromium Steel
Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4..