Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Notched | 0.583 J | 0.430 ft-lb | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |