Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.290 J/cm - NB | 0.543 ft-lb/in - NB | Average value: 11.4 J/cm Grade Count:26 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Unnotched | 0.290 J/cm | 0.543 ft-lb/in | ASTM Data |
Styron CALIBREâ„¢ 5101 15 Polycarbonate, 10% Glass Reinforced CALIBRE 5101 is a 10% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5101 resin exhibits high modulus and excellent dimensional stability. CALIBRE 5101 .. |