Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.441 J/cm
0.827 ft-lb/in
ASTM D256
Hyosung Topilene C600Y PP
C600Y Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.441 J/cm
0.827 ft-lb/in
ASTM D256
Hyosung Topilene J301CP PP
J301CP Injection Special Purpose GradeApplications: Cap of pressure bottleCharacteristics:High stiffnessSlip propertyInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.441 J/cm

@Temperature -10.0 °C
0.827 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene J640A PP
J640A Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporatio..
Izod Impact, Unnotched 0.441 J/cm

@Temperature -10.0 °C
0.827 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene J742 PP
J742 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporat..
Izod Impact, Unnotched 0.441 J/cm

@Temperature -10.0 °C
0.827 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene R200P PP
R200P Extrusion Random CopolymerApplications:Underfloor heating pipeWater service pipeCharacteristics:Pressure resistanceHigh impactLong-term heat stabilityFlexibilityInformation provided by Hyosung..
Izod Impact, Unnotched 0.441 J/cm

@Temperature -10.0 °C
0.827 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene J742S PP
J742S Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corpora..