Izod Impact, Unnotched 0.497 - 13.3 J/cm
0.930 - 25.0 ft-lb/in
Average value: 6.94 J/cm Grade Count:7
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Unnotched 0.497 J/cm
0.930 ft-lb/in
ASTM D256
Spartech PETG 3D Lenticular 3-D Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.497 J/cm
0.930 ft-lb/in
ASTM D256
Spartech APET SP4110 Copolyester Sheet
Description: Copolyester SheetInformation provided by Spartech.