Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.350 - 0.600 J/cm
0.656 - 1.12 ft-lb/in
Notch Status Unknown
Goodfellow Polyhydroxybutyrate - Biopolymer PHB
PHB and its copolymers with polyhydroxyvalerate (PHV) are melt-processable semi-crystalline thermoplastics made by biological fermentation from renewable carbohydrate feedstocks. They have been desc..