Polymer Property : Izod Impact, Unnotched = 1.31 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.31 J/cm
2.45 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific)
White colored thermally conductive mineral filled PA6 FR compound
Izod Impact, Unnotched 1.31 J/cm
2.45 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.