Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Unnotched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
North Wood Plastics HDPE with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |