Polymer Property : Izod Impact, Unnotched = 1.44 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.33 - 1.44 J/cm
2.49 - 2.70 ft-lb/in
Average value: 1.38 J/cm Grade Count:3
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched 1.33 - 1.44 J/cm
2.49 - 2.70 ft-lb/in
ASTM D256
Daikin NEOFLON M-300H PCTFE Granular Molding Powder
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by..
Izod Impact, Unnotched 1.33 - 1.44 J/cm
2.49 - 2.70 ft-lb/in
ASTM D256
Daikin NEOFLON M-300P PCTFE Pellets
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries.
Izod Impact, Unnotched 1.33 - 1.44 J/cm
2.49 - 2.70 ft-lb/in
ASTM D256
Daikin NEOFLON M-400H PCTFE Granular Molding Powder
NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process..