Polymer Property : Izod Impact, Unnotched = 1.65 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.65 - 3.74 J/cm
3.09 - 7.01 ft-lb/in
Average value: 2.55 J/cm Grade Count:7
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Izod Impact, Unnotched 1.65 J/cm
3.09 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 1.65 J/cm
3.09 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 684 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..
Izod Impact, Unnotched 1.65 J/cm
3.09 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 627 Nylon 6/6, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.