Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.95 J/cm | 3.65 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |