Polymer Property : Izod Impact, Unnotched = 10.18 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 10.18 J/cm
19.07 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized.