Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.35 J/cm | 11.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES (Asia Pacific) LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 6.37 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Unnotched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RF006Q PA 66 LNP* Thermocomp* RF006Q is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Reduced Moisture.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Unnotched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RF006Q PA 66 (Asia Pacific) LNP* Thermocomp* RF006Q is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Reduced Moisture.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Izod Impact, Unnotched | 6.37 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Unnotched | 6.36 J/cm | 11.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.37 J/cm @Thickness 3.17 mm |
11.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |