Mechanical Properties Metric English Comments
Izod Impact, Unnotched 60.0 J/cm

@Thickness 3.20 mm
112 ft-lb/in

@Thickness 0.126 in
ASTM D256
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM
15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
Izod Impact, Unnotched 60.0 J/cm

@Thickness 3.20 mm
112 ft-lb/in

@Thickness 0.126 in
ASTM D256
E-Polymers TEKAMID® TA210G15 , 15% Glass Fiber Reinforced PA66, DAM
Beautiful surface, strength propertyInformation provided by E-Polymers Co. Ltd.