Mechanical Properties Metric English Comments
Izod Impact, Unnotched 13.1 J/cm
24.5 ft-lb/in
ASTM D-4812
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Unnotched 13.1 J/cm
24.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC
LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare
Izod Impact, Unnotched 13.1 J/cm
24.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66
LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized.