Polymer Property : Izod Impact, Unnotched = 13.8 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 13.8 J/cm
25.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS
LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated.