Polymer Property : Izod Impact, Unnotched = 15.11 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 15.11 J/cm

@Temperature 23.0 °C
28.31 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl HS1000X PPE+PS
PPE+PS blend. 13% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL 746C f1. Radiant Panel listing. Dielectric strength. Dimensional stability. Suitable for ..