Izod Impact, Unnotched 0.834 - 8.70 J/cm
1.56 - 16.3 ft-lb/in
Average value: 3.24 J/cm Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..