Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Izod Impact, Unnotched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Izod Impact, Unnotched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Izod Impact, Unnotched | 9.61 J/cm @Temperature 23.0 °C |
18.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific) 40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Izod Impact, Unnotched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF30 HR HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and Hydrolysis ResistantFeatures: Heat Stabilized and Hydrolys.. |
|||
Izod Impact, Unnotched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Hydrolysis Resistant Appearance: .. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 7203-28 28% Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 7203-28 is a low profile, 28% glass reinforced polyester Sheet Molding Compound designed for automotive structural vehicle body panel applications that require high flexura.. |