Polymer Property : Izod Impact, Unnotched = 2.06 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.06 J/cm

@Thickness 3.17 mm
3.86 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Trirex® 3500G30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..