Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.1 J/cm | 20.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Unnotched | 11.1 J/cm | 20.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 (Asia Pacific) LNP* Lubricomp* RN001S is a compound based on Nylon 66 resin containing MOS2. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Izod Impact, Unnotched | 11.1 J/cm @Temperature 23.0 °C |
20.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10 LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas .. |
|||
Izod Impact, Unnotched | 11.1 J/cm | 20.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RC008 PA 66 LNP THERMOCOMP* RC008 is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 11.1 J/cm @Thickness 3.18 mm |
20.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Unnotched | 11.1 J/cm @Temperature 23.0 °C |
20.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10 (Asia Pacific) LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |